维普中文期刊产品整合服务
16篇 您的检索式:作者名="Hannoyer"
    题名 作者 年代 出处 被引量
1Transverse approach between real world concentrations of SO_2, NO_2, BTEX, aldehyde emissions and corrosion in the Grand Mare tunnel显示文摘With regard to automotive traffic, a tunnel-type semi enclosed atmosphere is characterized by a higher concentration of gaseous pollutants than on urban traffic roads and highlights the gaseous effluent species having an impact on material degradation. Therefore, a transverse approach between air quality and its consequences upon the longevity of materials is necessary, implying better knowledge of tunnel atmosphere and a better understanding of material degradation inside a tunnel for operating administration. Gaseous pollutant measurements carried out in a road tunnel in Rouen (Normandy) give the real world traffic concentrations of experimental exposure conditions. The sampling campaigns, achieved in summer and winter include SO2, NO2, BTEX and aldehyde analyses. Effluent profiles in the upward and downward tubes have been established. The current work shows that SO2, NO2, formaldehyde, acetaldehyde, propanal and butanal must be considered in the degradation process of materials in a stuffy environment. As regards NO2, its concentration depends on the modification of the automotive fleet. The total aldehyde concentrations indicate no particular trend between the two bores. Formaldehyde, acetaldehyde, propanal, butanal and acrolein species are the most abundant species emitted by vehicles and represent 90% to 95% of the total aldehyde emissions.I. Ameur-Bouddabbous J. Kasperek A. Barbier F. Harel B. Hannoyer 2012Journal of Environmental Sciences2012,24,7:2
2Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction analyses of mineral and organic matrix during heating of mother of pearl (naere) from the shell of the mollusc Pinetada maxima 显示文摘Balmain J Hannoyer B Lopez E 1999J Biomed Mater Res1999,48,5:1
3Non-destructive surface analysis applied to atmospheric corrosion of tin 显示文摘JOUEN S HANNOYER B PIANA O 2003Surface and Interface Analysis2003,34,:1
4Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction analysis of mineral and organic matrix during heating of mother of pearl (nacre) from the shell of the mollusk Pinctada Maxima 显示文摘 Hannoyer B Lopez E 1999J Biomed Mater Res1999,48,5:1
5Influence of substrate surface conditions on the plasma sprayed ceramic and metallic particles flattening显示文摘Syed A A Denoirjean A Hannoyer B 2005Surface and Coatings Technology2005,200,7:1
6Fourier Transform Infrared Spectroscopy (FTIR) and X-ray Diffraction Analyses of Mineral and Organic Matrix during Heating of Mother of Pearl (Nacre) from the Shell of the Mollusc Pinctada maxima显示文摘Balmain J Hannoyer B Lopez E 0,,:1
7Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction analyses of mineral and organic matrix during heating of mother of pearl (nacre) from the shell of the mollusc Pinctada maxima显示文摘Balmain J Hannoyer B Lopez E 1999J Biomed Mater Res1999,48,5:1
8Fourier transform infrared spectroscopy (FTIR) and X ray diffraction analyses of mineral and organic matrix during heating of mother of pearl (nacre) from the shell of the mollusc Pinctada maxima显示文摘BALMAIN J HANNOYER B LOPEZ E 1999J Biomed Mater Res1999,48,5:1
9Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction analyses of mineral and organic matrix during heating of mother of pearl (nacre) from the shell of the mollusc Pinctada maxima显示文摘Balmain J Hannoyer B Lopez E 1999Journal of Biomedical Materials Research1999,48,5:1
10Influence of substrate surface conditions on the plasma sprayed ceramic and metallic particles flattening 显示文摘Syed A A Denoirjean A Hannoyer B 2005Surface and Coatings Technology2005,,200:1
11Simultaneous Copper Runoff and Copper Surface Analysis in an Outdoor Area显示文摘JOUEN S JEAN M HANNOYER B 2000Surface and Interface Analysis2000,30,:1
12Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction analyses of mineral and organic matrix during heating of mother of pearl(nacre) from the shell of the mollusk Pinctada maxima显示文摘Balmain J Hannoyer B Lopez E 1999J Biomed Mater Res1999,48,5:1
13Effect of metal particles oxidation during the APS on the wettability显示文摘ESPIE G FAUCHAIS P HANNOYER P 1999Annals of the New York Academy of Sciences1999,891,:1
14Non-destructive surface analysis applied to atmospheric corrosion of tin显示文摘JOUEN S HANNOYER B PIANA O 2002Surface and Interface Analysis2002,34,1:1
15Initial stages of oxidation of Inconel 718 by FTIR spectroscopy显示文摘LENGLET M GUILLAMET R LOPITAUX J HANNOYER B 1990Materials Research Bulletin1990,25,6:1
16Simultaneouscopper runoff and copper surface analysis in an outdoor area显示文摘JOUEN S JEAN M HANNOYER B 2000Surface and Interface Analysis2000,30,:1
返回顶部 每页显示:
共1页 首页 上一页 第1页 下一页 末页 /1 跳转

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费